Page 97 - 南京医科大学学报自然科学版
P. 97
第41卷第7期 汤海燕,张 璐,陆 韬,等. 新型三维打印镁合金支架的显微结构及降解性能研究[J].
2021年7月 南京医科大学学报(自然科学版),2021,41(07):1021-1027 ·1027 ·
ed bone regeneration or left for spontaneous healing[J]. [15] 张智诚,田 君. Nd、Zr元素对铸造医用镁合金组织及
Clin Oral Implants Res,2017,28(3):348-354 耐蚀性能的影响研究[J]. 东莞理工学院学报,2020,27
[2] SEIBERT J S. Reconstruction of deformed,partially eden⁃ (5):78-83
tulous ridges,using full thickness onlay grafts. Part Ⅱ. [16] YANG C,YUAN G,ZHANG J,et al. Effects of magne⁃
Prosthetic/periodontal interrelationships [J]. Compend sium alloys extracts on adult human bone marrow⁃derived
Contin Educ Dent,1983,4(6):549-562 stromal cell viability and osteogenic differentiation[J].
[3] ELGALI I,OMAR O,DAHLIN C,et al. Guided bone re⁃ Biomed Mater,2010,5(4):045005
generation:materials and biological mechanisms revisited [17] SHEN Y,LIU W,LIN K,et al. Interfacial pH:a critical
[J]. Eur J Oral Sci,2017,125(5):315-337 factor for osteoporotic bone regeneration[J]. Langmuir,
[4] WESSING B,LETTNER S,ZECHNER W. Guided bone 2011,27(6):2701-2708
regeneration with collagen membranes and particulate [18] WITTE F,KAESE V,HAFERKAMP H,et al. In vivo cor⁃
graft materials:a systematic review and meta⁃analysis[J]. rosion of four magnesium alloys and the associated bone
Int J Oral Maxillofac Implants,2018,33(1):87-100 response[J]. Biomaterials,2005,26(17):3557-3563
[5] KHOJASTEH A,KHEIRI L,MOTAMEDIAN S R,et al. [19] SHAO S Y,CHEN J X,TANG H Y,et al. A titanium sur⁃
Guided bone regeneration for the reconstruction of alveo⁃ face modified with zinc⁃containing nanowires:enhancing
lar bone defects[J]. Ann Maxillofac Surg,2017,7(2): biocompatibility and antibacterial property in vitro[J].
263-277 Appl Surf Sci,2020,515:146107
[6] RAKHMATIA Y D,AYUKAWA Y,FURUHASHI A,et [20] SHAO S Y,MING P P,QIU J,et al. Modification of a SLA
al. Current barrier membranes:titanium mesh and other titanium surface with calcium⁃containing nanosheets and
membranes for guided bone regeneration in dental appli⁃ its effects on osteoblast behavior[J]. RSC Adv,2017,7
cations[J]. J Prosthodont Res,2013,57(1):3-14 (11):6753-6761
[7] BOYNE P J. Restoration of osseous defects in maxillofa⁃ [21] MING P P,SHAO S Y,QIU J,et al. Superiority of calcium
cial casualities[J]. J Am Dent Assoc,1969,78(4):767- ⁃ containing nanowires modified titanium surface com⁃
776 pared with SLA titanium surface in biological behavior of
[8] 温湘源,郑秋宝,詹潇锐,等. 拓扑优化设计结合 3D 打 osteoblasts:a pilot study[J]. Appl Surf Sci,2017,416:
印技术在骨科金属内植物的应用进展[J]. 中国临床解 790-797
剖学杂志,2020,38(6):745-748 [22] GU X N,ZHOU W R,YF Z,et al. Corrosion fatigue beha⁃
[9] SCHILLING T,BAUER M,BISKUP C,et al. Engineering viors of two biomedical Mg alloys ⁃ AZ91D and WE43 ⁃ in
of biodegradable magnesium alloy scaffolds to stabilize simulated body fluid[J]. Acta Biomater,2010,6(12):
biological myocardial grafts[J]. Biomed Tech(Berl), 4605-4613
2017,62(5):493-504 [23] 李 欢,文九巴,贺俊光,等. Mg⁃Zn⁃Zr系生物镁合金研
[10] 牛京喆,孙中刚,常 辉,等. 3D 打印医用钛合金研究 究现状及展望[J]. 材料热处理学报,2019,40(7):1-9
进展[J]. 稀有金属材料与工程,2019,48(5):1697- [24] 王欣宇,韩颖超,李世普,等. 羟基磷灰石仿骨结构材料
1706 制备及影响因素研究[J]. 硅酸盐通报,2003,22(2):
[11] 王淑琴,殷淑娟,许建霞,等. 纯镁在不同腐蚀体系中的 93-95
降解行为研究[J]. 药物分析杂志,2013,27(4):701- [25] 王亚明,邹永纯,王树棋,等. 金属微弧氧化功能陶瓷涂
705 层设计制备与使役性能研究进展[J]. 中国表面工程,
[12] 邬 波,柳 椰,马 旭,等. 3D 打印胶原/羟基磷灰石 2018,31(4):20-45
支架对骨髓间充质干细胞成骨分化的作用研究[J]. 中 [26] 韦宝伟,刘布鸣. 聚乳酸乙醇酸的生物降解和安全性研
华老年骨科与康复电子杂志,2020,6(3):123-127 究进展[J]. 现代药物与临床,2012,27(4):422-428
[13] LEE H,LIM C H,LOW M J,et al. Lasers in additive manu⁃ [27] LI X,CHU C,WEI Y,et al. In vitro degradation kinetics
facturing:a review[J]. Int J Precis Eng Manuf ⁃ Green of pure PLA and Mg/PLA composite:effects of immersion
Tech,2017,4(3):307-322 temperature and compression stress[J]. Acta Biomater,
[14] FURUKAWA M,IWAHASHI Y,HORITA Z,et al. Struc⁃ 2017,48:468-478
tural evolution and the hall⁃petch relationship in an Al⁃Mg [28] 韦雅玲. 镁合金/PLA 复合材料的制备与降解性能[D].
⁃ Li ⁃ Zr alloy with ultra ⁃ fine grain size[J]. Acta Mater, 南京:东南大学,2016
1997,45(11):4751-4757 [收稿日期] 2020-11-26